Ceramic coating was fabricated on Ti-6Al-4V alloy by micro-arc oxidation (MAO) at the constant current density of 6 A/dm2 in NaAlO2-Na3PO4 solution.

  • 在NaAlO2-Na3PO4电解液中于恒流条件下对Ti-6Al-4V合金进行了微弧氧化处理。