For ultra-hlgh strength steels after the closure of the hydrogen induced delay- ed plastic deformation zones,the SCC were nucleated at their tips.
英
美
- 对强度较低的钢,随滞后塑性变形的发展,应力腐蚀裂纹沿着滞后塑性区边界向前扩展。