Microstructure and fractography for the specimens of X80 pipeline steel chargied with hydrogen in constant load tests and in slow strain rate tests(SSRT)were studied by optical microscopy and SEM.
英
美
- 用光学显微镜和扫描电镜观察了不同充氢电流下恒载荷拉伸试样、慢应变速率拉伸试样的显微组织和断口形貌。