On the other hand, utilizing Rapid Thermal Processing (RTP) system, SiNWs were prepared on the same substrates as above.
英
美
- 另外,通过1150℃和1200℃下30s的快速热处理(Rapid Thermal Processing,RTP),在镀金硅衬底上生长出SiNWs。