Propagation develops within the working surface of the roll, gradually increasing in depth and width followed by a large surface spall of the overlying barrel surface.
英
美
- 这种断裂首先是在工作层中产生的,进而逐渐往辊身方向变深变宽,最终导致辊身大面积的剥落。