The ICT scan results indicated that the joint zone of the condenser baffle,condenser tubes and the welds are the sites suffered from serious corrosion damage.

  • ICT扫描分析结果表明;在列管、管板和焊材的结合区域腐蚀最为严重;盐水侧的管板腐蚀呈蜂窝状;而液氯侧的孔蚀较盐水侧严重.