The air entrapment of the liquid metal flow in the shot sleeve during the slow shot phase is one of the factors resulting in this kind of defect.
英
美
- 气孔是压铸生产中的常见问题,导致这一缺陷的原因之一就是在慢压射过程中压室内的金属液流动卷入了气体。