The cause of the ballrace craze of our product was analyzed by means of fractography,metallographic examination,ingredient analyses,electron microscope analyses and rigidity detection,etc.

  • 采用断口分析、金相检验、成份分析、电镜分析和硬度检测等方法对某产品用的滚道分析了产生裂纹的原因。