The effect of cyclic stress on the strength of creep rupture and recurrent creep rupture as well as low cycle fatigue of a cast nickel-base superalloy with high Al and Ti contents has been studied under different temperature and stress.
英
美
- 本文对一种高铝钛镍基铸造合金,在不同温度分别测定单调持久、周期持久和低周疲劳性能。