The effect of melt superheating treatment on the microstructure and stress rupture properties of M963 superalloy under the condition of 1248 K/225 MPa has been investigated.
英
美
- 对M963合金熔体进行了过热处理并在1248 K/225 MPa条件下测试了其持久性能.