The effects of crystal orientation and pulling rate on the liquid-solid interface morphology in the directional solidification of DD8 nickel-base superalloy have been investigated.
英
美
- 研究了DD8镍基高温合金定向凝固界面形态的晶体取向及抽拉速度的影响。