The formation and aggravation of hydrogen damage in Fe-3wt-%Si alloy during cathodic charging were studied by means of Lange transmission X-ray topography.

  • 采用Lange式透射X射线形貌照相法研究了电解充氢导致Fe-3wt-%25Si单晶中氢损伤的规律。