The long afterglow luminescent material of Sr_2MgSi_2O_7 was prepared by sintering at high temperature under the deoxidization atmosphere.

  • 首先,采用高温固相法,在还原气氛下制备出Sr_2MgSi_2O_7基长余辉发光材料。