The results showed that the HAZ impact toughness decreased with the increase in peak temperature and hence the fractographic appearance changed from dimple pattern to cleavage or quasi-cleavage pattern.

  • 结果表明,随着峰值温度的提高,冲击韧性下降,断口形貌由韧窝状变成解理或准解理状。