The results showed that the adding of appropriate active agent(stearate) during the grind process can reduce the glass powder size and size distribution.
英
美
- 结果表明,在玻璃粉的制备过程中,加入适量的活性剂(硬脂酸盐),可以大大降低玻璃粉的粒径和粒径分布范围。