The single crystal superalloy DD3 was joined by TLP diffusion bonding with an interlayer alloy of XH4A,which was specially designed for DD3.
英
美
- 为了实现DD3单晶合金叶片的优质连接,采用专为DD3设计的XH4A中间层合金,对DD3进行了TLP扩散焊试验。