Thermomechanical fatigue(TMF) life of three temperature-strain phase angles and two specimen dimensions was studied in directional solidification(DS) superalloy DZ125.
英
美
- 对DZ125定向凝固铸造镍基高温合金进行了三种相位和两种试样尺寸的热机械疲劳实验研究。