the necessary condition and resolvent on inert metal anodes maden by superalloy for aluminium electrolysis are discussed;and the correlative trends and orientation of study are introduced.
英
美
- 阐述适用于铝电解工业的惰性阳极合金所应具备的必要条件和必须解决的问题,并介绍目前有关的研究动态和研究方向。